Influences Of A Thermal Tempering Process On Radial Crack Formation By Indentation In Plate Glass

The threshold load for radial crack formation on Vickers indentation was measured for soda-lime glass slides with different degrees of thermal toughening that gave a range of surface compression stresses.

Author
R Dal Maschio Et Al
Origin
Trento, Padua, Massachusetts Univs, Staz Sper Del Vetro, Murano
Journal Title
Phys Chem Glasses 1989 30 2 59-61