Influence Of Tank Depth And Throughput On Flow In Glass Tank Furnaces (In German)

A study has been made of flow in a glass furnace based on a mathematical model for 2-dimensional temperature and velocity distributions along the tank. Examination of the results leads to the recommendation that tank depth should be decreased and additional energy introduced in the batch-melting region.

Author
G. Leyens And J. Smecek
Origin
Unknown
Journal Title
Glastechnische Berichte 1982 24 (26) 81-87