Industrial Minerals And Rocks In Sweden

In 1994, the production of industrial minerals and rocks in Sweden was 9.6m tonnes, with an unprocessed value of Skr 1,100m. (1,100m Swedish Crowns). A calculated processed value would be more than Skr 6,000m.