Industrial Glassmelting Process Analysis: Part 1 Modular Melting

The difference between the minimum residence time versus average residence time, the high amount of energy absorption in the initial stages of melting and the importance of energy flux to the batch blanket in current melting processes are studied by partioning the melting process into functional modules.

Author
R Beerkens
Origin
Tno, Netherlands
Journal Title
Am Ceramic Soc Bull 83 4 2004 28-32
Sector
General
Class
G 2788