Industrial Gases For Crystal Glass Manufacture

This paper reviews the main applications of industrial gases used in crystal glass manufacture.

Author
L Philippe & T Huchet
Origin
Air Liquide, France
Journal Title
Verre 5 4 1999 25-28
Sector
Domestic glass
Class
D 425