Individual Oxy-Fuel Benefits Should Be Clear Before Conversion

Specific applications may be unique or very different from other conversions. However, glass manufacturers with no previous oxy-fuel experience require a clear understanding of how oxy-fuel will benefit their furnaces and processes prior to conversion.