[India] Waste Glass Geared At Construction

Refuse glass bottles from laboratories can now be used in construction works under a recycling process designed by the Central Marine Fisheries Research Institute (CMFRI) as part of its Swatchhata initiative. Under the new waste management initiative, the CMFRI has set up a glass crushing unit that will pulverise them into sand-like shreds which could be used for construction works, the Institute announced in a press release recently. Other types of glass can also be crushed, such as tubes, lights etc.