Improving Glass Conditioning

The Zedtech forehearth uses air dampers, a patented Rapid Cool technology and Low Forward Velocity (LFV) burners to give improved temperature homogeneity of the glass, higher pulls and a wider tonnage range compared with other types of forehearths.