Improving Annealing Regimes For Curved Glass Units During Bending

An optimal schedule has been developed for annealing glass at three constant cooling panels. This has enabled the cooling rate of a glass panel to be doubled compared with the conventional schedules based on the Adams and Williamson equations.

Author
V I Puchugin, A V Fedotov, V M Braude
Origin
Unknown
Journal Title
Glass And Ceramics 1988 45 1-2 20-22