Improvements In Or Relating To The Manufacture Of Flat Glass.

The manufacture of thin flat glass on a molten metal support by providing a reaction to traction right across the width of the molten glass from which a glass ribbon is being drawn. The process is especially adapted to the production of very thin flat glass and glass foil (down to 0.005mm).