The flow of a viscous liquid thorough a channel and nose feeder was studied using a physical model. An equation has been derived which can be used for automatic gob weight control by tube rotation .
Origin
Unknown
Journal Title
Glastechnische Berichte 1983 56K (1) 136-140
Sector
Primary Papers
Class
PP 703