How One Glass Company Gains A Cullet Supply From Community Collection Programme

The involvement of the Foster Forbes Division of American National Can Co. in the Carolinas Glass Recycling Programme is described.

Author
S Grisham
Origin
Unknown
Journal Title
American Glass Review February 1988 7-8