How A Mass Heat Extractor Can Increase The Pull Rate Of A Forehearth

This article shows what happens by changing the zoning of a particular design and the manner in which it is operated.

Author
M Stanley & C H Viel
Origin
Bh-F (Eng) Ltd, Uk & St Goabin Emballage (France)
Journal Title
Glass Industry 75 11 1994 28-31
Sector
Container glass
Class
C 731

Request article (free for British Glass members)

How A Mass Heat Extractor Can Increase The Pull Rate Of A Forehearth
Glass Industry 75 11 1994 28-31
C 731