Hollow Glassware Toughening Considerations

The technology and advantages of toughening as applied to tumblers and saucers are described briefly.

Author
N Porfido
Origin
Cnud Sa
Journal Title
Glass International December 1989 45, 47
Sector
Domestic glass
Class
D 75