High Pressure Benefits Of Waterjet Cutting

The abrasive jet cutting system has become an established tool for the flat glass processor. According to Esab-Hancock GmbH, this is unlikely to replace conventional methods for many applications, the technology offers an economically attractive solution in other important areas.

Author
Un-named
Origin
Esab-Hancock Gmbh
Journal Title
Glass 70 6 1993 241-242