High-Precision Powder Application

A high-precision jet powder application system, manufactured by HU Platsch KG of Stuttgart, has been successfully introduced into the glass industry. Thousands of these powdering units have been used for many years in the graphical industry and in the paper and plastic converting industries. With this system, separating mediums such as Lucite, Lignocell, Colacryl, Separol, nut shell and other powders can be applied in very fine dosage and, more importantly, with high homogeneity.