[Heye International] Swabbing Robot Enhances Productivity And Operator Safety

All four high speed Tandem IS machines at Ardagh's Moerdijk glass container plant near Rotterdam have been equipped with specially developed robots to perform essential mould swabbing duties. The Ardagh Glass project team responsible for this innovative technology worked closely with Heye and robotics specialist Socabalec to create a system that provides significant productivity and cost saving benefits. The project is discussed in more detail in this article.