Glazing As An Integral Part Of Car Evolution

Very much in evidence at the 1999 Frankfurt Motor Show, from the glazing point of view, were technological advances which fit in with overall developments of the car. In this paper the author illustrates this concept by looking at progress in electronics, alternative fuels, active and passive safety as well as opportunities for new materials with regard to transparent roofs, sunroofs and materials for encapsulation.

Author
G Manfre
Origin
Mg Consult, Italy
Journal Title
Glass-Tech Int 1/2000 151-157
Sector
Flat glass
Class
F 1101