Glass Strength And Frame - Whose Problem Is It?

John Weir, standards secretary for the Glass & Glazing Federation, explains the full implications of Section 5.11 of BS 6262 and the effect of the appearance of Part 1 of the proposed CEN standard for insulating glass units.