Three billion plastic drinking straws end up in the trash each day, after a single use. This is now a thing of the past with Schott Straws. Schott Straws for hotels and restaurants, as well as for private households, are made from the same glass as drinking glasses and can be reused between 1000-2000 times. For safety reasons, the wall thickness of the glass tubes is 1.5mm. This makes them more robust than conventional drinking glass, i.e. they don't break in your mouth or in the dishwasher.