Glass Quality: What To Expect From Fused Cast Refractory

A degradation mechanism in fusion cast refractories subjected to very high stresses, especially in the presence of thermal variations, is described.

Author
P C Ratto
Origin
Refel
Journal Title
Glass Production Technology International 1991 41-44