Glass Lightweighting - Trends And Environmental Benefits

The development of lighter, stronger glass bottles is one of the most important factors in the continued success of glass packaging. Modern Narrow-Neck Press and Blow (NNPB) techniques for beverage, sauce and spirit bottle production are capable of reducing bottle weights by up to 20%.