Glass Furnace Technology For Reduced Emissions Based On Advanced Control And Monitoring

This paper reports an advanced furnace viewing sensor for regenerative U-flamed glass furnaces, which is demonstrated in a 40t/d pull furnace of tableware glass burning thick fuel oil. The system processes digitized images from the combustion chamber and uses information related to the geometric features of the flame for monitoring furnace performance. The procedure is shown to be able to reduce NOx levels by up to 20%, by means of adequate control of the fuel atomization air.

Author
D Correia Et Al
Origin
Inst Superior Tecnico, Lisbon, Portugal
Journal Title
Glastech Ber Glass Sci Technol 69 10 1996 305-310
Sector
General
Class
G 1530

Request article (free for British Glass members)

Glass Furnace Technology For Reduced Emissions Based On Advanced Control And Monitoring
Glastech Ber Glass Sci Technol 69 10 1996 305-310
G 1530
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.