The Glass Factories Of The 18Th Century (In Italian)

This essay is the last from ten which are part of the unpublished collection "Vita Quotidiana dei Muranesi del Settecento", where the author has made an attempt to reconstruct, year by year, the events - not only those strictly connected to the glass factories - of the Muranese people. His studies are based exclusively on extant documents of the State Archives of Venice, the manuscripts at the Correr Library and the Glass Museum in Murano, and on the registers of the four parishes of the island.

Author
S Tagliapietra
Origin
Unknown
Journal Title
Rivista Della Staz Sper Del Vetro 26 1 1996 33-37
Sector
General
Class
G 1456

Request article (free for British Glass members)

The Glass Factories Of The 18Th Century (In Italian)
Rivista Della Staz Sper Del Vetro 26 1 1996 33-37
G 1456
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.