Glass Decoration By The Thermal Fusion Process

The advantages of transfers applied by the thermal fusion process are discussed briefly.

Author
F L Barnes
Origin
Capper Ratuad Ltd
Journal Title
Glass February 1988 56
Sector
Flat glass
Class
F 44