Glass Decoration - The Importance Of Colour

With pressure for lead and cadmium free enamles increasing in recent years, the market for organic paints and inks which are cured at low temperature such as those manufactured by Fluorital, has been growing. This article looks at the benefits of these types of products, such as quick color change and low temperature requirements, and explains how they can be applied in different sectors of the market.

Author
A Gozo
Origin
Fluorital, Italy
Journal Title
Gmpa 5/99 118-122
Sector
Domestic glass
Class
D 434