Glass Decoration Elements History And Technology

This paper is about the testing of different glass decorations elements which belong to historical items, in order to retrieve information about their history and technology of production. The research was carried out on small pieces of glass borrowed from historical objects in partnership between AGH (Technical University of Science & Technology) and four different conservator groups. Testing was carried out by non-destructive techniques.