Glass Corrosion Effects From Dishwashing And Their Technical Solution

Glass corrosion from automatic dishwashing has been investigated by atomic force microscopy (AFM) and other surface sensitive methods. The results show completely different basic causes of glass attack. Local clouding at the mouth rim or line corrosion can be traced back to the production process of the glass. Components of cleaning agents were found to be responsible for iridescence and clouding all over. The comprehensive knowledge of the corrosion mechanism was used to establish one possible technical solution to avoid glass corrosion. Using the so-called Protector Dual Protection, the cleanness and brilliance of glass can be conserved even if the glass passed many cycles in automatic dishwashing. The mechanism to prevent the glass surface and enamels are described in this paper, which can be downloaded in full from: www.db-thueringen.de/servlets/DerivateServlet/Derivate-30968/ilm1-2014iw...

Author
Dr D Werner
Origin
Technical University Iimenau
Journal Title
58Th Ilmenau Scientific Colloquium September 2014
Sector
Domestic glass
Class
D 1372

Request article (free for British Glass members)

Glass Corrosion Effects From Dishwashing And Their Technical Solution
58Th Ilmenau Scientific Colloquium September 2014
D 1372
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.