Glass Conditioning - What Is It And How Do We Achieve It?

Optimising the combustion and cooling systems are the keys to forehearth design philosophy.

Author
J Mcminn
Origin
Parkinson Spencer, Uk
Journal Title
Glass Industry 81 1 2000 30-32
Sector
Container glass
Class
C 1567