Glass In Building - Global Activity On Standards And Regulation

Standardization as it relates to glass in buildings has seen progress in recent years with technical committees CEN TC and ISO TC 160, as well as their working groups, operating both together and individually. This article details the latest work of these two groups and explains the relationship between the standards emerging and EU requirements.

Author
J B Waldron
Origin
Pilkington, Uk
Journal Title
Glass-Tech Int 2/2000 145-149