Glass Artists And Their Personal Opinions And Viewpoints

This article is based on an interview with three important names in artistic glass: Alessandro Lenarda, Giusto Toso, and the young designers of Design Juice Studio. They were asked to respond to four fundamental questions on the creation of artistic glass objects, with reference to the Igloo brand.