Getting The Best Of Both Worlds

Glaverbel's Moustier plant in Belgium, the world's largest flat glass plant, has installed a unique plant to recover the dust from gas flue scrubbing. The dust, made up predominantely of sulphates, is recycled as a raw material, achieving the objective of zero waste.

Author
Un-named
Origin
Unknown
Journal Title
Glass & Glazing Products Sept 1998 44
Sector
Flat glass
Class
F 871