German Innovation In Colour Sorting Technology

The German engineering firm, S & S Metallsuchgerate, has developed a colour sorting system for cullet capable of handling up to 15 tonnes/h at a working width of 1200mm. The system also separates out non-transparent contaminants and cullet covered with labels.