Gepvp Code Of Practice For In-Situ Measurement And Evaluation Of The Colour Of Coated Glass Used In Facades

This Code of Practice describes a method for allowing an objective evaluation of the colour of coated glass, as defined in EN 1096-1, when used in facades. It provides a method for measuring colour differences within the same glass pane and between two adjacent panes in the same facade. Specific requirements are given for coated glass, dependent upon its light transmittance and reflectance. Guidance is also provided on angle dependency, reflection from interior and transmission.

Author
Un-named
Origin
Unknown
Journal Title
Gepvp January 2005 (Available To Download From Gepvp Website)
Sector
Flat glass
Class
F 3013

Request article (free for British Glass members)

Gepvp Code Of Practice For In-Situ Measurement And Evaluation Of The Colour Of Coated Glass Used In Facades
Gepvp January 2005 (Available To Download From Gepvp Website)
F 3013
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.