Gas Recovery Systems For Float Glass Lines

This article takes a look at how Netherlands-based HyGear is developing a recycling system to recover the hydrogen and nitrogen from the tin bath of float glass lines. The opportunities lie in the reduction of operational utility costs (hydrogen and nitrogen). Therefore, the system fits well with the glass industry's aim of energy and cost savings.

Author
Un-named
Origin
Unknown
Journal Title
Glass International May 2015 41-42
Sector
Flat glass
Class
F 3679