Future Possibility Of High Performance Pvb Interlayer: Multi-Layer Technology For Noise Reduction And More

Recent automotive glazing requires various functions such as comfort, security & environmental impact in addition to safety. In order to meet customers' demands, PVB for laminated glass plays an important role in high performance automotive glazing. In this article, multi-layer technology of PVB interlayer is presented as a superior solution for high performance glazing. Particularly, sound control interlayer will be discussed to show how multi-lyaer technolgoy contributes to a higher level of performance glazing. Maximum sound attenuation level could never be achieved with singer layer acoustic PVB film because of its low mechanical strength & handling difficulties. Unlike single layer acoustic film, sound attenuation performance in multi-layer PVB construction can be optimised to maximum level by having different functions in the outer and inner layer.

Author
T Yoshioka
Origin
Sekisui Chemical Co Ltd
Journal Title
Glass Processing Days 2003 525-527
Sector
Flat glass
Class
F 1688

Request article (free for British Glass members)

Future Possibility Of High Performance Pvb Interlayer: Multi-Layer Technology For Noise Reduction And More
Glass Processing Days 2003 525-527
F 1688
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
16 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.