The Future Of Glass Melting

Advances in combustion technologies for glass processing was the theme of a workshop hosted by the Glass Manufacturing Industry Council (GMIC) in February this year. Overall, 150 delegates met in Washington, DC, to discuss the need for energy efficient, lower cost, higher productivity furnace designs.

Author
Un-named
Origin
Unknown
Journal Title
Glass Int May/June 2001 23-24
Sector
General
Class
G 2382

Request article (free for British Glass members)