Fused-Cast Cruciform Technology

SEPR has been developing cruciforms for regenerator packing since 1973. The latest atage in the evolution of these products is for borosilicate application. This technology combines high density material and a special variable thickness to improve chemical resistance in the borate component. This paper describes the history of the company's cruciform products and a brief description of the latest advances.