[Furnaces] Optimelt Set To Reduce Emissions At Libbey'S Oxy-Fuel Fired Furnace

This article discusses the implementation of Praxair's Optimelt system at Libbey's Leerdam plant in The Netherlands. The system was originally installed at Pavisa's container glass site in Mexico with successful results. The Optimelt thermochemical regenerator (TCR) heat recovery system provides a compelling solution to maximise heat recovery from oxy-fuel fired glass furnaces to improve energy efficiency and to minimise furnace emissions.

Author
J De Diego Et Al
Origin
Praxair, Spain
Journal Title
Glass International July-August 2017 75-76, 78
Sector
Domestic glass
Class
D 1417

Request article (free for British Glass members)

[Furnaces] Optimelt Set To Reduce Emissions At Libbey'S Oxy-Fuel Fired Furnace
Glass International July-August 2017 75-76, 78
D 1417
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
7 + 13 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.