Furnace Operations - Siad And Falorni: Air-Oxygen-Natural Gas Combusion For Artistic Glass Production

This article presents a new combustion system in response to the needs of glassmakers regarding production processes, reaching maximum furnace operation. This innovative technical proposal, developed by Siad and Falorni Glass Furnaces, has already been applied in several kinds of furnaces for artistic glass production with benefits that are illustrated here.

Author
F Dentella & P Zucca
Origin
Siad Spa, Italy
Journal Title
Gmpa 5/05 92-95
Sector
Domestic glass
Class
D 875