Furnace Conceptions And Energy Supply

As energy prices increase, it is vital for energy-intensive industries to find optimum use for the energy resources available. This article explains how Horn, of Germany, is using its R&D department to research furnace design and its influence on energy consumption. Statements and comparisons concerning the specific energy consumption of individual furnaces are given.

Author
C Jatzwauk
Origin
Horn Industries, Germany
Journal Title
Glass Worldwide Sept-Oct 2007 40, 42-44