Functional Laminated Glazing Of Passenger Vehicles By Advanced Pvb Technology - Multi-Layer Technology For Noise Reduction And More

The functions required for automotive glazing are becoming more diverse to meet customer needs such as comfort, security, and environmental issues in addition to safety. PVB interlayer for laminated glass is being discussed more as a practical way of adding new functions on the automotive glass system.

Author
T Yoshioka
Origin
Sekisui Chemical Co, Japan
Journal Title
Int Glass Review 2/2003 73-77
Sector
Flat glass
Class
F 1444