Fuel Saving Through Glass Selection

This paper discusses the advantages of heat resistant automotive glass when it comes to saving on fuel consumption.

Author
Dr R Farrington & J Rugh
Origin
Nat Renewable Energy Labs, Usa
Journal Title
Asian Glass Feb-Mar/04 48-49
Sector
Flat glass
Class
F 1493