[France] Innovative Solutions For A Vital Process

This article discusses SGD Pharma's innovative solutions for implementing aseptic filling with ready-to-use moulded glass vials.

Author
C Grassi
Origin
Sgd Pharma
Journal Title
Glass Worldwide Jan-Feb 2020 54-56