Fragility And Local Structure Of Agi-Ag20-B203 Glasses

Viscosities and thermal properties of glasses in the system AgI-Ag20-B203 were investigated in the temperature region of the glass transformation.

Author
S K Lee Et Al
Origin
Osaka Prefecture University, Japan
Journal Title
Phys Chem Glasses 38 3 1997 144-147
Sector
Special Glass
Class
S 1179

Request article (free for British Glass members)

Fragility And Local Structure Of Agi-Ag20-B203 Glasses
Phys Chem Glasses 38 3 1997 144-147
S 1179
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.