Formation Features Of Thin Float Glass And Prospects For This Technology (A Review)

The principal methods for producing thin float glass are identified based on an analysis of patent information. Brief descriptions of patented methods are given. The problems of formation of tin float glass and ways of solving them are considered. Promising directions in the production of thin float glass are described.