Focused Approach To Container Production Expansion

Within the past decade, the fortunes of Brazilian glass container producer Vidroporto have been transformed. This article summarises an interview with Edson Rossi, President of the company, about the changes made and the involvement of Container Glass Alliance member companies in the completion in 2014 of a third production shop.