Fluorosulfuric Acid As A Raw Material For The Acid Polishing Process

The improvement potential of fluorosulphuric regeneration in the acid polishing process in the lead crystal industry is demonstrated by several model calculations. Successful conversion of a two-batch polishing plant from conventional to HSO3F regeneration is described.

Author
A Kaiser
Origin
Fraunhofer-Institut Fur Silicatforschung
Journal Title
Glastech Ber 1989 62 4 127-134
Sector
Domestic glass
Class
D 63