Fluorescence Of Atomic Silver In Glasses And Crystals

Metal atoms represent a group of fluorescent enters which have the advantage of known structure. Due tot their neutrality, they are not affect by their surroundings.

Author
W.A. Weyl Et Al.
Origin
Unknown
Journal Title
J. Electrochem. Soc., 95 [2] 70-79 (1949)