Flow Of Molten Glass Through And Open Channel.

The flow of molten glass through an open channel of uniform rectangular cross section is examined theoretically. For fluid of uniform viscosity, several analytical solutions are available. These cannot be applied to molten glass since wide variations in temp are to be expected and the viscosity of glass strongly depends on temp.

Author
G.E. Hearn And F. Booth
Origin
Unknown
Journal Title
Glass Technol., 15 [3] 81-86 1974